Phase-specific properties in a low-alloyed TRIP steel investigated using correlative nanoindentation measurements and electron microscopy

Download (1.47 MB)
journal contribution
posted on 2024-11-16, 06:05 authored by Zhiping Xiong, Ahmed Saleh, Gilberto Casillas-Garcia, Shaogang Cui, Elena PerelomaElena Pereloma
Nanoindentation measurements of polygonal ferrite (PF), bainitic ferrite (BF) lath, ferrite in granular bainite (GB) and retained austenite (RA) in a low-alloyed multi-phase transformation-induced plasticity steel were carried out in conjunction with electron backscattering diffraction and scanning transmission electron microscopy (STEM). PF returned the lowest hardness followed by ferrite in GB, BF lath and RA. Dislocation glide and austenite-to-martensite transformation can be correlated with the first and second pop-in observed in the load-displacement curve, respectively. The martensite transformation induced by nanoindentation was demonstrated via correlative STEM. Film RA generally shows a higher stability than blocky RA, associated with a larger average onset load for martensite transformation in the former. It is noted that some ferrite in GB had similar hardness to BF lath and some blocky RA grains in GB showed a similar stability to that of film RA between BF lath, which can be attributed to a higher carbon content in GB due to chemical inhomogeneity.

Funding

Focused ion beam microscope for trace element analysis and nanomachining

Australian Research Council

Find out more...

An analytical field emission gun scanning electron microscope

Australian Research Council

Find out more...

History

Related Materials

  1. 1.
    ISSN - Is published in 0022-2461

Citation

Xiong, Z., Saleh, A. A., Casillas, G., Cui, S. & Pereloma, E. V. (2020). Phase-specific properties in a low-alloyed TRIP steel investigated using correlative nanoindentation measurements and electron microscopy. Journal of Materials Science, 55 (6), 2578-2587.

Journal title

Journal of Materials Science

Volume

55

Issue

6

Pagination

2578-2587

Language

English

RIS ID

139767

Usage metrics

    Categories

    Keywords

    Exports

    RefWorks
    BibTeX
    Ref. manager
    Endnote
    DataCite
    NLM
    DC